Inshine E702
Product Features
A high cut-off ultraviolet EVA film, and glass and other materials with good adhesion. To ensure the safety of the operation of components and long-term anti-aging and has a UV cutoff function.



Product characteristics
Test items |
unit |
Referenced standards |
Specification value |
|
Wide in width |
mm |
GB/T 13542.2-2009 |
standard value(0-+5) |
|
Weight in grams |
g/m2 |
ISO 536-2012 |
≥ standard value |
|
Tensile strength(MD) |
MPa |
GB/T 13542.2-2009 |
≥16 |
|
Tensile strength(TD) |
MPa |
GB/T 13542.2-2009 |
≥16 |
|
Elongation at break(MD) |
% |
GB/T 13542.2-2009 |
≥550 |
|
Elongation at break(TD) |
% |
GB/T 13542.2-2009 |
≥550 |
|
Heat shrinkage rate(120℃×3min)MD |
% |
GB/T 13542.2-2009 |
≤3.0 |
|
Heat shrinkage rate(120℃×3min)TD |
% |
GB/T 13542.2-2009 |
≤0.5 |
|
EVA and Backboard Peel Strength |
N/cm |
GB/T 2790-1995 |
≥60 |
|
EVA and glass peel strength |
N/cm |
GB/T 2790-1995 |
≥80 |
|
Transmittance(380-1100nm) |
% |
T/CPIA0004-2017 |
≥90 |
|
Transmittance(380-290nm) |
% |
T/CPIA0004-2017 |
≤30 |
|
Volume resistivity |
Ω·cm |
GB/T 1410-2006 |
≥1×1015 |
|
Breakdown voltage intensity (AC method) |
KV/mm |
GB/T 1408.1-2016 |
≥25 |
|
CTI |
V |
GB/T 4207-2012 |
≥400 |
|
Crosslinking degree (xylene method) |
% |
GB/T 29848-2013 |
≥75 |
|
Constant damp heat test 85℃×85%RH 1000H |
Yellowing index△YI |
-- |
IEC 61215-2 2016 |
≤5.0 |
Peel strength with glass |
N/cm |
≥40 |
||
UV aging resistance test 120KWH/m2 |
Yellowing index△YI |
-- |
IEC 61215-2 2016 |
≤5.0 |
Peel strength with glass |
N/cm |
≥40 |
||
PCT high temperature and high humidity experiment 48h |
Yellowing index△YI |
-- |
T/CPIA0004-2017 |
≤5.0 |
Peel strength with glass |
N/cm |
|
≥40 |